Fixing Conditions (Heat Press)

The conditions under which you must fix the ink with a heat press differ between White ink and color ink. Make sure that you meet these conditions for fixing the ink.

Optimum conditions vary depending on the type of heat press. Test and check the results in advance to determine the correct pressure.

Ink type Time Temperature Pressure
Color 45 seconds 338 °F (170 °C) 6 Psi (4.2 N/cm2)
White
Larger than A4 size with White ink Up to 90 seconds
Note: If the ink is not completely dry after 90 seconds, extend the duration while carefully checking if the pre-treatment solution is dry.